Inconel 625 datasheet
Inconel 625 Datasheet
:
: 58-69%
: 20-23%
: 8-10%
: 3.15-4.15%
: 5%
: 0.4%
: 0.4%
: 0.5%
: 0.5%
: 0.5%
: 0.1% (max)
: 0.015% (max)
: 0.015% (max)
:
: 8.44 g/cm³ (8440 kg/m³)
: 1,300 degree to 1,400 degree (2,372 degree F to 2,552 degree F)
:
11.2 W/m·K (at 100 degree )
:
0.42 J/g·K (at 100 degree )
: 930 MPa (135,000 psi)
: 240 MPa (35,000 psi)
: 30% (in 2 inches)
(Brinell): 200-250 HB
: 200 GPa (29 × 10⁶ psi)
:
: Excellent at high temperatures up to 1,000 degree (1,832 degree F).
: High resistance to SCC in high-stress, high-temperature environments.
:
: Nuclear reactors, high-temperature power plant components.
:
: Can be forged, hot-rolled, and cold-rolled.
: Typically solution-annealed at 1,010 degree (1,850 degree F) and rapidly cooled.
:
ASTM B446: Standard specification for Inconel 625.
AMS 5666: Aerospace specification for Inconel 625 bars, billets, and forgings.
DIN 17744: German standard for Inconel 625 products.
Inconel 625 and its essential properties, making it suitable for high-performance applications in extreme environments.